The metal is first cast into mushroom-shaped ingots and then cooled by ambient temperature. It then.

The metal is
first cast into mushroom-shaped ingots and then cooled by ambient temperature.
It then is rolled successively (up to 14 times), with water cooling the metal
with each pass through the rolling mill. Special care is taken to roll the
bronze at a different angle with each pass, to minimize anisotropy, impart
preferred grain orientation, and develop an even, round shape.