The H13 tool-steel mold is preheated 200° to 450°C, depending on the cast alloy and part size….

The H13
tool-steel mold is preheated 200° to 450°C, depending on the cast alloy and
part size. Initially, preheat is achieved with a hand-held torch, but after a
few castings, the mold reaches a steady state temperature profile.